Manufacturer: RADICI
Produced At: Europe / China
Product Category: Polyamide 6 (Nylon 6)
Product No: Radilon BN 200 AS/2
Product Quantity: 25KG / BAG
Product Features: Crystalline,Good Flow,Medium Viscosity
Radilon? BN 200 AS/2
Flame Rated
Crystalline
Medium Viscosity
Features |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
Density | 1.13 | -- | g/cm3 | ISO 1183 |
Water Absorption 2 (Equilibrium, 73°F, 0.0394 in, 50% RH) | 2.7 to 3.3 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
Tensile Modulus | 435000 | 174000 | psi | ISO 527-2/1A/1 |
Tensile Stress (Yield) | 12300 | 7250 | psi | ISO 527-2/1A |
Tensile Strain (Yield) | 4.0 | 20 | % | ISO 527-2/1A |
Flexural Modulus 3 | 363000 | 145000 | psi | ISO 178 |
Flexural Stress 3 | 10200 | -- | psi | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
Charpy Notched Impact Strength(73°F) | 3.8 | -- | ft·lb/in2 | ISO 179/1eA |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-22°F | 48 | -- | ft·lb/in2 | |
73°F | No Break | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
Heat Deflection Temperature | ||||
66 psi, Unannealed | 320 | -- | °F | ISO 75-2/B |
264 psi, Unannealed | 149 | -- | °F | ISO 75-2/A |
Melting Temperature 4 | 428 | -- | °F | ISO 3146 |
Flammability | Dry | Conditioned | Test Method | |
Flame Rating | HB | -- | UL 94 |
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields