Manufacturer: DSM
Produced At: Europe / China
Product Category: Thermoplastic Copolyester Elastomer
Product No: Arnitel EB463
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized
Arnitel? EB463
Heat stabilized or stable to heat
Boots and Bellows
Additive |
|
Features |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
Density | 1.15 | g/cm3 | ISO 1183 |
Melt Volume-Flow Rate (MVR) (230°C/10.0 kg) | 0.641 | in3/10min | ISO 1133 |
Water Absorption | ISO 62 | ||
Saturation, 73°F | 0.70 | % | |
Equilibrium, 73°F, 50% RH | 0.30 | % | |
Hardness | Nominal Value | Unit | Test Method |
Shore Hardness (Shore D, 3 sec) | 38 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
Tensile Modulus | 9430 | psi | ISO 527-2 |
Tensile Stress | ISO 527-2 | ||
Break 2 | 3480 | psi | |
Break | 2610 | psi | |
5.0% Strain 2 | 493 | psi | |
5.0% Strain | 508 | psi | |
10% Strain 2 | 798 | psi | |
10% Strain 3 | 769 | psi | |
10% Strain | 870 | psi | |
10% Strain, 212°F 3 | 406 | psi | |
50% Strain 2 | 1200 | psi | |
50% Strain | 1670 | psi | |
100% Strain 2 | 1290 | psi | |
100% Strain | 2180 | psi | |
Tensile Strain 2 (Break) | 810 | % | ISO 527-2 |
Nominal Tensile Strain at Break | 200 | % | ISO 527-2 |
Elastomers | Nominal Value | Unit | Test Method |
Tear Strength 4, 5 | 1300 | lbf/in | ISO 34-1 |
Impact | Nominal Value | Unit | Test Method |
Charpy Notched Impact Strength | ISO 179/1eA | ||
-22°F | No Break | ||
73°F | No Break | ||
Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-22°F | No Break | ||
73°F | No Break | ||
Notched Izod Impact Strength | ISO 180/1A | ||
-4°F | No Break | ||
73°F | No Break |
Thermal | Nominal Value | Unit | Test Method |
Melting Temperature 6 | 397 | °F | ISO 11357-3 |
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields