Manufacturer: DSM
Produced At: Europe / China
Product Category: Nylon 66(PA66)
Product No: Akulon S223-EH
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized、Low Viscosity、Lubricated、Medium Viscosity
Akulon? S223-EH
Heat stabilized or stable to heat
Low viscosity
Lubricated
Medium viscosity
Additive |
|
Features |
|
Processing Method |
|
Multi-Point Data |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
Density | 1.14 | -- | g/cm3 | ISO 1183 |
Molding Shrinkage | ISO 294-4 | |||
Across Flow | 1.6 | -- | % | |
Flow | 1.6 | -- | % | |
Water Absorption | ISO 62 | |||
Saturation, 73°F | 8.5 | -- | % | |
Equilibrium, 73°F, 50% RH | 2.3 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
Tensile Modulus | 508000 | 218000 | psi | ISO 527-2 |
Tensile Stress (Yield) | 13800 | 8700 | psi | ISO 527-2 |
Tensile Strain (Yield) | 3.5 | 20 | % | ISO 527-2 |
Nominal Tensile Strain at Break | 25 | > 50 | % | ISO 527-2 |
Flexural Modulus | 406000 | -- | psi | ISO 178 |
Flexural Stress | 18100 | -- | psi | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
Charpy Notched Impact Strength | ISO 179/1eA | |||
-22°F | 2.9 | 2.9 | ft·lb/in2 | |
73°F | 2.9 | 5.7 | ft·lb/in2 | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-22°F | No Break | No Break | ||
73°F | No Break | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
Heat Deflection Temperature | ||||
66 psi, Unannealed | 437 | -- | °F | ISO 75-2/B |
264 psi, Unannealed | 176 | -- | °F | ISO 75-2/A |
Melting Temperature 3 | 500 | -- | °F | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 5.6E-5 | -- | in/in/°F | |
Transverse | 5.6E-5 | -- | in/in/°F | |
Effective Thermal Diffusivity | 4.87E-8 | -- | m2/s |
Electrical | Dry | Conditioned | Unit | Test Method |
Volume Resistivity | 1.0E+14 | 1.0E+12 | ohms·cm | IEC 60093 |
Electric Strength | 640 | 510 | V/mil | IEC 60243-1 |
Relative Permittivity | IEC 60250 | |||
100 Hz | 3.40 | 10.0 | ||
1 MHz | 3.20 | 4.00 | ||
Dissipation Factor | IEC 60250 | |||
100 Hz | 0.013 | 0.30 | ||
1 MHz | 0.020 | 0.10 | ||
Comparative Tracking Index | 600 | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
Flammability Classification | IEC 60695-11-10, -20 | |||
0.06 in | V-2 | -- | ||
0.028 in | HB | -- |
Fill Analysis | Dry | Conditioned | Unit | |
Melt Density | 0.969 | -- | g/cm3 | |
Melt Thermal Conductivity | 0.90 | -- | Btu·in/hr/ft2/°F | |
Specific Heat Capacity of Melt | 0.657 | -- | Btu/lb/°F |
Injection | Dry | Unit | |
Drying Temperature | 176 | °F | |
Drying Time | 4.0 to 8.0 | hr | |
Rear Temperature | 509 to 545 | °F | |
Middle Temperature | 527 to 554 | °F | |
Front Temperature | 536 to 563 | °F | |
Nozzle Temperature | 536 to 554 | °F | |
Processing (Melt) Temp | 518 to 563 | °F | |
Mold Temperature | 122 to 176 | °F | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 435 to 1450 | psi | |
Screw Compression Ratio | 2.5:1.0 |
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields