Manufacturer: Envalior/DSM
Produced At: Europe / China
Product Category: Nylon 6(PA6)
Product No: Akulon K224-HG6U
Product Quantity: 25KG / BAG
Product Features: Heat Stabilized,Lubricated
Akulon? K224-HG6U
Polyamide 6
Contains release agent
Heat stabilized or stable to heat
Lubricated
Filler / Reinforcement |
|
Additive |
|
Features |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
Density | 1.38 | -- | g/cm3 | ISO 1183 |
Water Absorption | ISO 62 | |||
Saturation, 73°F | 6.3 | -- | % | |
Equilibrium, 73°F, 50% RH | 1.9 | -- | % |
Mechanical | Dry | Conditioned | Unit | Test Method |
Tensile Modulus | 1.45E+6 | 957000 | psi | ISO 527-2 |
Tensile Stress (Break) | 26100 | 16000 | psi | ISO 527-2 |
Tensile Strain (Break) | 3.5 | 5.0 | % | ISO 527-2 |
Flexural Modulus | 1.33E+6 | -- | psi | ISO 178 |
Flexural Stress | 36300 | -- | psi | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
Charpy Notched Impact Strength | ISO 179/1eA | |||
-22°F | 5.2 | 5.2 | ft·lb/in2 | |
73°F | 7.1 | 14 | ft·lb/in2 | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-22°F | 36 | 33 | ft·lb/in2 | |
73°F | 45 | 52 | ft·lb/in2 |
Thermal | Dry | Conditioned | Unit | Test Method |
Heat Deflection Temperature | ||||
66 psi, Unannealed | 428 | -- | °F | ISO 75-2/B |
264 psi, Unannealed | 410 | -- | °F | ISO 75-2/A |
Melting Temperature 3 | 428 | -- | °F | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 1.1E-5 | -- | in/in/°F | |
Transverse | 3.9E-5 | -- | in/in/°F | |
Effective Thermal Diffusivity | 1.13E-7 | -- | m2/s |
Electrical | Dry | Conditioned | Unit | Test Method |
Volume Resistivity | 1.0E+14 | 1.0E+12 | ohms·cm | IEC 60093 |
Electric Strength | 760 | 640 | V/mil | IEC 60243-1 |
Relative Permittivity | IEC 60250 | |||
100 Hz | 3.50 | 20.0 | ||
1 MHz | 3.30 | 5.00 | ||
Dissipation Factor | IEC 60250 | |||
100 Hz | 5.0E-3 | 0.30 | ||
1 MHz | 0.015 | 0.12 | ||
Flammability | Dry | Conditioned | Unit | Test Method |
Flammability Classification | IEC 60695-11-10, -20 | |||
0.028 in | HB | -- | ||
0.06 in | HB | -- |
Fill Analysis | Dry | Conditioned | Unit | |
Melt Density | 1.20 | -- | g/cm3 | |
Melt Thermal Conductivity | 2.0 | -- | Btu·in/hr/ft2/°F | |
Specific Heat Capacity of Melt | 0.511 | -- | Btu/lb/°F |
Injection | Dry | Unit | |
Drying Temperature | 176 | °F | |
Drying Time | 4.0 to 8.0 | hr | |
Rear Temperature | 491 to 509 | °F | |
Middle Temperature | 509 to 527 | °F | |
Front Temperature | 509 to 536 | °F | |
Nozzle Temperature | 500 to 536 | °F | |
Processing (Melt) Temp | 482 to 545 | °F | |
Mold Temperature | 122 to 176 | °F | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 435 to 1450 | psi | |
Screw Compression Ratio | 2.5:1.0 |
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields