Manufacturer: TORAY
Produced At: Japan / China
Product Category: PA66
Product No: Amilan U320
Product Quantity: 25KG / BAG
Product Features: High Impact Resistance
Amilan? U320
Features |
|
Uses |
|
Part Marking Code |
|
Physical | Dry | Conditioned | Unit | Test Method |
Density (73°F) | 1.09 | -- | g/cm3 | ISO 1183 |
Molding Shrinkage - Across Flow 3(0.118 in) | 1.2 to 1.5 | -- | % | Internal Method |
Water Absorption | ISO 62 | |||
73°F, 24 hr | 1.1 | -- | % | |
Saturation, 73°F | 6.0 | -- | % | |
Hardness | Dry | Conditioned | Unit | Test Method |
Rockwell Hardness (R-Scale, 176°F) | 114 | -- | ISO 2039-2 |
Mechanical | Dry | Conditioned | Unit | Test Method |
Tensile Stress | ISO 527-2 | |||
-40°F | 14500 | 13300 | psi | |
73°F | 8700 | 6240 | psi | |
Tensile Strain | ISO 527-2 | |||
Break, -40°F | 5.5 | 8.5 | % | |
Break, 73°F | 30 | 50 | % | |
Flexural Modulus | ISO 178 | |||
-40°F | 377000 | 377000 | psi | |
73°F | 290000 | 116000 | psi | |
Flexural Stress | ISO 178 | |||
-40°F | 16700 | 16000 | psi | |
73°F | 10900 | 5800 | psi | |
Taber Abrasion Resistance (1000 Cycles) | 7.00 to 8.00 | -- | mg | ISO 9352 |
Impact | Dry | Conditioned | Unit | Test Method |
Charpy Notched Impact Strength | ISO 179 | |||
-40°F | 6.7 | 9.5 | ft·lb/in2 | |
73°F | 10 | 27 | ft·lb/in2 |
Thermal | Dry | Conditioned | Unit | Test Method |
Heat Deflection Temperature | ||||
66 psi, Unannealed | 356 | -- | °F | ISO 75-2/B |
264 psi, Unannealed | 140 | -- | °F | ISO 75-2/A |
Melting Temperature | 509 | -- | °F | DSC |
CLTE - Flow | 5.6E-5 to 6.1E-5 | -- | in/in/°F | ISO 11359-2 |
Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields